Enhanced piezoelectric properties of (Bi0.5Na0.5)1-xBax TiO3 lead-free ceramics by sol-gel method

Zhao Ming-Lei Wang Chun-Lei Wang Jin-Feng Chen Hong-Cun Zhong Wei-Lie

Enhanced piezoelectric properties of (Bi0.5Na0.5)1-xBax TiO3 lead-free ceramics by sol-gel method

Zhao Ming-Lei, Wang Chun-Lei, Wang Jin-Feng, Chen Hong-Cun, Zhong Wei-Lie
PDF
Get Citation

(PLEASE TRANSLATE TO ENGLISH

BY GOOGLE TRANSLATE IF NEEDED.)

Metrics
  • Abstract views:  2997
  • PDF Downloads:  862
  • Cited By: 0
Publishing process
  • Received Date:  08 February 2003
  • Accepted Date:  08 August 2003
  • Published Online:  15 July 2004

Enhanced piezoelectric properties of (Bi0.5Na0.5)1-xBax TiO3 lead-free ceramics by sol-gel method

  • 1. 山东大学物理与微电子学院,晶体材料国家重点实验室,济南 250100

Abstract: The dielectric, piezoelectric, ferroelectric and pyroelectric properties of (Bi0.5Na0.5)1-xBaxTiO3 (x=0.00,0.04,0.06,0.08, 0.12) ceramics prepared by sol-gel method were investigated. It was found that all the samples in this experiment show improved piezoelectric properties,obtained by using this chemical method. For(Bi0.5Na0.5)0.94Ba0.06TiO3 ceramic, as its composition is near the morphotropic phase boundary (MPB), it shows the largest piezoelectric constant, d33=173×10-12C/N, which is about 40% improvement compared to the conventional processed ceramics in this system. In addition, from the ferroelectric and pyroelectric measurements, the remanent polarization Pr, coercive field Ec and depolarization temperature Td of the (Bi0.5Na0.5)0.94Ba0.06TiO3 ceramic were found to be 25μC/cm2, 28kV/cm, and 80℃, respectively.