用计算机控制的自动倒扭摆测量了轻度冷加工的铝-0.5wt%铜合金试样在室温(20℃)时效24小时后的自由衰减曲线。此时的内耗值虽然很低,但在逐次增加激发振幅进行内耗测量时也观察到一系列的振幅内耗峰。Free decay curves of slightly cold-worked Al-0.5 wt% Cu specimen aged at room temperature (20℃) for 24 hrs were determined by an automatic inverted torsion pendulum with computer control. A series of amplitude internal friction peaks were observed as the excitation amplitude was increased succestively even when the internal friction was very low.