由观测无胁强作用下的热膨胀和电阻研究金属玻璃(Fe0.85Ni0.15)84B16的结构弛豫

CSTR: 32037.14.aps.37.1855

STUDY OF THE STRUCTURAL RELAXATION OF METALLIC GLASS (Fe0.85Ni0.15)84B16 BY MEASURING THE THERMAL EXPANSION AND RESISTANCE UNDER ZERO STRESS

CSTR: 32037.14.aps.37.1855
PDF
导出引用
  • 本文通过长度、电阻和热膨胀系数的测量研究了(Fe0.85Ni0.15)84B16金属玻璃结构弛豫和退火温度Ta的关系。基于上述物理量对结构弛豫的关系,对曲线作了分析和讨论。在退火温度为175℃至250℃之间结构弛豫随Ta的变化率最大。

     

    The dependence of the structural relaxation of the material on the annealing temperature Ta is studied by measuring the difference of thermal elongation △l or that of the electrical resistivity △ρ and that of the thermal expansion coeffcient △α between an as-quenched and an annealed sample. △α/α0 is measured by placing an as-quenched and an annealed sample in juxtaposition and heating them with iodine-tungsten lamps. The samples expand freely and the rsitivity of the as-onerched sample, respeomparator. The experimental results are summarized by three curves, namely △α/α0 vs Ta, △l/l0 vs Ta and △ρ/ρ0 vs Ta, where α0, l0, and ρ0 are the linear expansion coefficient, the length and the resistivity of the as-quenched sample, respec lively. The obtained results are discussed.

     

    目录

    /

    返回文章
    返回